The buried layer within these metal-in static shield zipper bags won't rub off or remove with chemicals, like IPA, thanks to the film printing process per MIL-PRF-81705E standards. The bags measure 10 x 14in and come in a 100-pack.
The buried layer within these metal-in static shield zipper bags won't rub off or remove with chemicals, like IPA, thanks to the film printing process per MIL-PRF-81705E standards. The bags measure 10 x 14in and come in a 100-pack.
This features standard stock bags that are converted per MIL-DTL-117H.
Features
| Tensile Strength | Typical Value: 4,600psi, 32mPa; Testing Method: ASTM D882 | 
| Puncture Resistance | Typical Value: 12lbs, 53N; Testing Method: MIL-STD-3010 Method 2065 | 
| Seam Strength | Typical Value: Pass; Testing Method: MIL-STD-3010 Method 2024 | 
| Thickness | Typical Value: 2.8mils, 0.071mm ±10%; Testing Method: MIL-STD-3010 Method 1003 | 
| Marking Abrasion Resistance | Typical Value: Pass; Testing Method: MIL-PRF-81705E Method 4.6.6 | 
| Contact Corrosivity | Typical Value: Pass; Testing Method: MIL-STD-3010 Method 3005* | 
| Transparency | Typical Value: 40%; Testing Method: MIL-STD-3010 Method 4034 | 
| EMI Attenuation | Typical Value: ≥ 10dB; Testing Method: MIL-PRF-81705E Method 4.6.7 | 
| ESD Shielding | Typical Value: ≤ 10nJ; Testing Method: MIL-PRF-81705E Method 4.6.9 | 
| Surface Resistivity - Interior | Typical Value: ≥ 1 x 10&sup5; to < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E Method 4.6.8 | 
| Surface Resistivity - Exterior | Typical Value: < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E Method 4.6.8 | 
| Static Decay | Typical Value: ≤ 2 seconds; Testing Method: MIL-STD-3010 Method 4046 | 
| Temperature/td> | 360°F (182°C) | 
| Time | 2 seconds | 
| Pressure | 60psi, 414kPa | 
| Tensile Strength | Typical Value: 4,600psi, 32mPa; Testing Method: ASTM D882 | 
| Puncture Resistance | Typical Value: 12lbs, 53N; Testing Method: MIL-STD-3010 Method 2065 | 
| Seam Strength | Typical Value: Pass; Testing Method: MIL-STD-3010 Method 2024 | 
| Thickness | Typical Value: 2.8mils, 0.071mm ±10%; Testing Method: MIL-STD-3010 Method 1003 | 
| Marking Abrasion Resistance | Typical Value: Pass; Testing Method: MIL-PRF-81705E Method 4.6.6 | 
| Contact Corrosivity | Typical Value: Pass; Testing Method: MIL-STD-3010 Method 3005* | 
| Transparency | Typical Value: 40%; Testing Method: MIL-STD-3010 Method 4034 | 
| EMI Attenuation | Typical Value: ≥ 10dB; Testing Method: MIL-PRF-81705E Method 4.6.7 | 
| ESD Shielding | Typical Value: ≤ 10nJ; Testing Method: MIL-PRF-81705E Method 4.6.9 | 
| Surface Resistivity - Interior | Typical Value: ≥ 1 x 10&sup5; to < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E Method 4.6.8 | 
| Surface Resistivity - Exterior | Typical Value: < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E Method 4.6.8 | 
| Static Decay | Typical Value: ≤ 2 seconds; Testing Method: MIL-STD-3010 Method 4046 | 
| Temperature/td> | 360°F (182°C) | 
| Time | 2 seconds | 